awnl Posted June 9, 2015 Share Posted June 9, 2015 I had some interesting results while trying to make 415 do what I want. I was happy to see smooth creamy tops. TOMH your right, you will get different results depending on the temperature . Onto next challenge getting a strong HT . Quote Link to comment Share on other sites More sharing options...
HensleyLaure Posted June 9, 2015 Share Posted June 9, 2015 At what temp did you pour in order to get smooth tops? Quote Link to comment Share on other sites More sharing options...
awnl Posted June 9, 2015 Author Share Posted June 9, 2015 Between 100-110 Quote Link to comment Share on other sites More sharing options...
HensleyLaure Posted June 9, 2015 Share Posted June 9, 2015 Last time I used it, I poured at about 90 degrees, when it looked slushy. My tops turned out pretty smooth, but I'm always looking to have even better tops! Lol Quote Link to comment Share on other sites More sharing options...
awnl Posted June 9, 2015 Author Share Posted June 9, 2015 How your ht ? Quote Link to comment Share on other sites More sharing options...
HensleyLaure Posted June 9, 2015 Share Posted June 9, 2015 Really good, but I used 10% fo. Quote Link to comment Share on other sites More sharing options...
8-GRAN-ONES Posted June 9, 2015 Share Posted June 9, 2015 Great..it is fun to get them to turn out great the first time. .You can also hit then with a heat gun if for some reason the are not smooth. . Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.