bac Posted March 26, 2007 Share Posted March 26, 2007 I read the post on buldging with 1343..great results. I have a question. I'm using 4625 overpour with chunks made with 1343. I used 24 ply wick and got some buldging during my 5th burn. I really like the 24 ply since it leaves a shell..Do you think I can add a little stearic to the 4625 to make it a little harder? Other info: I'm using a square mold 3x3x4.5 and scent was cotton blossom..Does too much scent cause buldging? In my case I added 9% to 8 oz of wax. Thanks for your help. Bianela Quote Link to comment Share on other sites More sharing options...
grama Posted March 26, 2007 Share Posted March 26, 2007 I use the 4625 and use the 30ply and have very good results with it. Don't use any additive with this. Quote Link to comment Share on other sites More sharing options...
grama Posted March 26, 2007 Share Posted March 26, 2007 Forgot to add I use no more than 1.25 oz pp and on some fo use only .75 oz. Never go over 1.25 though. Quote Link to comment Share on other sites More sharing options...
bac Posted March 26, 2007 Author Share Posted March 26, 2007 I tried the 30 ply but it doesn't leave as much of a shell. I'm also trying 27ply. Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.