Margaritamama Posted September 18, 2005 Share Posted September 18, 2005 Is it possible to "rustic" 1274 wax, or does it have to be poured at the same temp in order to ensure a mottle effect? Quote Link to comment Share on other sites More sharing options...
topofmurrayhill Posted September 18, 2005 Share Posted September 18, 2005 It will mottle fine, but possibly a little less. The main factor for mottling is how much FO you put in. Pouring temp and cooling rate affect it but they're secondary.Basically anything you see people doing with 1343, you can do with 1274 also. Quote Link to comment Share on other sites More sharing options...
Margaritamama Posted September 18, 2005 Author Share Posted September 18, 2005 Thanks Top. I'm going to give it a bash and see how it works. Isn't that what it's all about - experimentation?!?!? Quote Link to comment Share on other sites More sharing options...
topofmurrayhill Posted September 18, 2005 Share Posted September 18, 2005 You got that right babe. Quote Link to comment Share on other sites More sharing options...
Margaritamama Posted September 18, 2005 Author Share Posted September 18, 2005 ........... Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.