TK81
-
Posts
2 -
Joined
-
Last visited
Content Type
Profiles
Articles
Media Demo
Forums
Gallery
Events
Store
Blogs
Downloads
Posts posted by TK81
-
-
so I've started making clamshells using 4826 tart wax. Once they cool I notice they are all dipping. I've tried pouring at cooler Temps(150-160) and warmer Temps (175-180). I've tried cooling racks and no cooling racks! What should I be doing? Can I just top them office? I'm so confused lol 😆
Thanks in advance!
TK
clamshells sinking
in Wickless
Posted
Thank you. I do use 6006 for candles that come out great. I might try that. I did have to do a 2nd pour on my last batch of clamshells. My prob with the 1st batch was that I completely filled them leaving little room to pour a 2nd.